| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D792 |
| Water Absorption | 0.020 % | 0.020 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 45 | 45 | ASTM D785 |
| Hardness, Rockwell R | 66 | 66 | ASTM D785 |
| Tensile Strength, Ultimate | 22.8 MPa | 3310 psi | ASTM D638 |
| Elongation at Break | >= 100 % | >= 100 % | ASTM D638 |
| Flexural Strength | 33.1 MPa | 4800 psi | ASTM D790 |
| Flexural Modulus | 1.20 GPa | 174 ksi | ASTM D790 |
| Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 11.7 J/cm | 21.9 ft-lb/in | ASTM D256 |
| Gardner Impact | 13.6 J | 10.0 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 160 °C | 320 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 77.0 °C | 171 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 49.0 °C | 120 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |