Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.45 g/cc Green Density

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer Ametek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.45 g/cc Green Density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
P409L/409CB is a ferritic, weldable grade of stainless steel high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and has the capacity to provide high-caliber mechanical properties due to the high-temperature sintering response. P409L/409CB’s versatility also results from Cb being less prone to oxidation than Ti. In addition, the oxide is unable to combine with carbon and the Cb forms a stable carbide which prevents coarsening of carbides and grains in the weld’s heat-affected zone. P409L/409CB may be used in automotive exhaust system applications, among other uses.For property data reported here: Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Compacting pressure 40 tsi. Green strength 1800 psi. Sintered breaking strength105,000 psi.Information provided by Ametek Specialty Metal Products.
Physical Properties Metric English Comments
Bulk Density 2.90 g/cc
0.105 lb/in³
Powder
Density 6.55 g/cc
0.237 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell B 71
71
Tensile Strength, Ultimate 372 MPa
54000 psi
Elongation at Break 4.8 %
4.8 %
Thermal Properties Metric English Comments
Shrinkage 0.28 %
0.28 %
versus die size
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 10.5 - 11.75 %
10.5 - 11.75 %
Iron, Fe 84.35 - 89.1 %
84.35 - 89.1 %
As Remainder
Manganese, Mn <= 2.0 %
<= 2.0 %
Niobium, Nb (Columbium, Cb) 0.40 - 0.80 %
0.40 - 0.80 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Descriptive Properties Value Comments
Powder Flow 30 sec/50 g