Material Notes:
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend allows for visual inspection of proper mixing and ratios. Shelf life: 12+ months (unmixed).Processing:100/(40-100) ratio. Pot life: 100 g, 30-40 min. at 25°C(77°F). Hardens in 3-5 hours at 25°C (77°F), 4-6 min. at 80°C (175°F), 2 min. at 120°C (250°F), 24 sec to 1 min. at 150°C (300°F).Corrosion Resistance: good resistance to atmospheric conditions, soft and salt water, alkalis and diluted acids.
Physical Properties Metric English Comments
Water Absorption 0.20 %
0.20 %
after 24 hrs.
Viscosity Measurement 200

@Temperature 25.0 - 27.0 °C
200

@Temperature 77.0 - 80.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
100/40 pbw; 68 at 100/80 pbw; 66 (60 after 10 sec) at 100/100 pbw
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Elongation at Break 3.0 %
3.0 %
Typical averaged test results for Abatron Adhesive/Casting Resins.
Flexural Yield Strength 83.0 MPa
12000 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Compressive Yield Strength 115 MPa
16700 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.