Abatron AboCast 8-22/Abocure 8-22 Epoxy  (discontinued **)

Category Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8-22/Abocure 8-22 Epoxy  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/55.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 23 hours at 20°C (68°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Viscosity Measurement 375

@Temperature 20.0 °C
375

@Temperature 68.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60