Aaron Industries AAROLENE® ARPP C 200-3 Polypropylene Compounded Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® ARPP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® ARPP C 200-3 Polypropylene Compounded Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Melt Flow 8.0 - 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 - 12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 35.5 MPa
5150 psi
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 3.74 J/cm
7.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
262 °F
ASTM D648