Applications: Aerospace Rivet Material; High Pressure Oxygenated Gas Vents; Superconducting Wire Information provided by ATI Wah Chang
Physical Properties Metric English Comments
Density 5.70 g/cc
0.206 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 546 MPa
79200 psi
Tensile Strength, Yield 480 MPa
69600 psi
Elongation at Break 23 %
23 %
in 1 in gage
Modulus of Elasticity 62.05 GPa
9000 ksi
Thermal Properties Metric English Comments
CTE, linear 9.03 µm/m-°C

@Temperature 20.0 °C
5.02 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 10.0 W/m-K
69.4 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Niobium, Nb (Columbium, Cb) 45 %
45 %
Titanium, Ti 55 %
55 %
Descriptive Properties Value Comments
Thermal Diffusivity, ft²/sec 46.3
Users viewing this material also viewed the following: