Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Centrex® 601 Profile Extrusion Grade AES

Category Polymer , Thermoplastic , AES Polymer , AES, Extruded
Manufacturer Diamond and Network Polymers
Trade Name Centrex®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Diamond Polymers Centrex® 601 Profile Extrusion Grade AES.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyvinyl chloride (PVC).Applications: Typical applications for Centrex 601 resin include exterior siding and window frames panels. As with any product, use of Centrex 601 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Melt Flow 6.0 g/10 min
<br>@Load 10.0 kg,<br> Temperature 230 °C
6.0 g/10 min
<br>@Load 22.0 lb,<br> Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.4 MPa
3390 psi
chs 2.0 in/min; ASTM D638
Tensile Strength, Yield 28.3 MPa
4100 psi
chs 2.0 in/min; ASTM D638
Tensile Modulus 1.722 GPa
249.8 ksi
chs 2.0 in/min; ASTM D638
Flexural Strength 44.1 MPa
6400 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 1.585 GPa
229.9 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.800 J/cm
<br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
1.50 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature -40.0 °F
ASTM D256
1.28 J/cm
<br>@Thickness 3.17 mm,<br> Temperature -18.0 °C
2.40 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature -0.400 °F
ASTM D256
5.34 J/cm
<br>@Thickness 3.17 mm,<br> Temperature 23.0 °C
10.0 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
ASTM D256
Impact Test 26.0 J
<br>@Temperature -40.0 °C
19.2 ft-lb
<br>@Temperature -40.0 °F
ASTM D3763
38.0 J
<br>@Temperature 23.0 °C
28.0 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
41.0 J
<br>@Temperature -18.0 °C
30.2 ft-lb
<br>@Temperature -0.400 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 28.0 µm/m-°C
15.6 µin/in-°F
ASTM D696
Optical Properties Metric English Comments
Gloss 50 - 70 %
50 - 70 %
Sheet/Profile; 60°; ASTM D523