Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Primacor® 5986 Ethylene acrylic acid copolymer

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings , Ethylene Acrylic Acid
Manufacturer Dow Chemical
Trade Name Primacor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Primacor® 5986 Ethylene acrylic acid copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low heat seal temperature High gloss, excellent clarity Excellent grease and oil resistance and excellent product resistance for flexible packaging applications Complies with U.S. FDA 21 CFR 177.1310 (c) PRIMACOR™ 5986 has excellent adhesion to metallic, cellulosic, glass and other polar substrates. It can be used effectively as a foil primer or laminating adhesive for polyethylene and metallized substrates. Information provided by Dow.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D792
Melt Flow 13.8 g/10 min

@Load 2.16 kg,
Temperature 125 °C
13.8 g/10 min

@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
Melt Index of Compound 300 g/10 min

@Load 2.16 kg,
Temperature 125 °C
300 g/10 min

@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
Compression molded; ASTM D2240
Tensile Strength at Break 9.65 MPa
1400 psi
Compression molded; ASTM D638
Elongation at Break 390 %
390 %
Compression molded; ASTM D638
Tensile Modulus 0.0331 GPa
4.80 ksi
2% Secant; Compression molded; ASTM D638
Thermal Properties Metric English Comments
Melting Point 77.2 °C
171 °F
Dow Method (DSC)
Vicat Softening Point 42.2 °C
108 °F
ASTM D1525
Descriptive Properties Value Comments
Comonomer content, % 20.5
measured by direct titration