Dow Corning SYL-OFF® PMCP7362 Coating

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® PMCP7362 Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Syl-Off® 7362 Coating is a 30% solids dispersion of vinyl functional silicone polymer in toluene. A pre-catalysed coating suitable for fast cure applications, recommended for use with 7367 Crosslinker.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc

@Temperature 25.0 °C
0.890 g/cc

@Temperature 77.0 °F
Viscosity 23000 cP
23000 cP
Dynamic
Thermal Properties Metric English Comments
Flash Point 4.40 °C
39.9 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 30
Color Clear, Slighty Hazy