Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Nextel™ XN-513 Woven Fabric 720

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer 3M
Trade Name Nextel™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Nextel™ XN-513 Woven Fabric 720.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by 3M
Physical Properties Metric English Comments
Density 3.40 g/cc
0.123 lb/in³
Permeability 20
20
[ft<sup>3</sup>/min/ft<sup>2</sup>], Air w/o sizing
Thickness 330 microns
13.0 mil
Fiber Count 1670 dtex
1500 denier
roving
Mechanical Properties Metric English Comments
Tensile Strength at Break 2100 MPa
305000 psi
filament 25.4mm
Tensile Modulus 248 GPa
36000 ksi
filament
Tear Strength 28.4 kN/m
162 pli
Warp, Breaking Strength w/o Sizing
28.4 kN/m
162 pli
Fill, Breaking Strength w/o Sizing
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 100 - 1100 °C
3.33 µin/in-°F

@Temperature 212 - 2010 °F
Melting Point 1800 °C
3270 °F
Optical Properties Metric English Comments
Refractive Index 1.67
1.67
Component Elements Properties Metric English Comments
Al2O3 85 %
85 %
SiO2 15 %
15 %
Electrical Properties Metric English Comments
Dielectric Constant 5.8

@Frequency 9.375e+9 Hz
5.8

@Frequency 9.375e+9 Hz
Users viewing this material also viewed the following: