| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 330 microns | 13.0 mil | |
|
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
Polystrand ThermoPro™ IE6021 ECR Unitape Unidirectional Polyethylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
|
|||
| Thickness | 330 microns | 13.0 mil | Total; ASTM D374 |
|
Parker Chomerics T-Wings Heat Spreaders
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade..
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
Parker Chomerics T-Wing™ Heat Spreader
Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. T-Wing spreaders consist of..
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
Polystrand ThermoBallistic™ TBS8010X X-Ply Cross-Ply Polypropylene-Glass Composite
2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoBallistic laminates combine continuous S-Glass (ThermoBallistic-S™) structural fibers with a proprietary polypropylene thermoplastic poly..
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
Hexcel® HexForce™ 2523 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
Hexcel® HexForce™ 383 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
|
|||
| Thickness | 330 microns | 13.0 mil | Nominal |
|
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness
Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: ..
|
|||
| Thickness | 330 microns | 13.0 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate..
|
|||
| Thickness | 330 - 432 microns | 13.0 - 17.0 mil | Overall |
|
Arlon 28941C015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Thickness | 330 - 432 microns | 13.0 - 17.0 mil | Overall |
|
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
|
|||
| Thickness | 330 - 432 microns | 13.0 - 17.0 mil | Side 1 |
|
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
|
|||
| Thickness | 330 microns | 13.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon 51112R013 0.013" (0.330 mm) Cured, Self Fusing, Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured, Self Fusing, Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data sho..
|
|||
| Thickness | 330 microns | 13.0 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon 55173R045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f..
|
|||
| Thickness | 330 microns | 13.0 mil | Side 2; Arlon SQA-TMS-003 |
|
Arlon 55173R045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f..
|
|||
| Thickness | 330 microns | 13.0 mil | 7500 Fiberglass, Substrate |
|
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info..
|
|||
| Thickness | >= 330 microns | >= 13.0 mil | Side 1 |
|
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, ..
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
3M Nextel™ AF-12 Aerospace Woven Fabric 312
Information provided by 3M
|
|||
| Thickness | >= 330 microns | >= 13.0 mil | Side 2 |
|
Arlon 51576R027 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
|
|||
| Thickness | 330 - 381 microns | 13.0 - 15.0 mil | Overall |
|
Arlon R31651R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
|
|||
| Thickness | 330 microns | 13.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic..
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
3M Nextel™ AF-12 Industrial Woven Fabric 312
Information provided by 3M
|
|||
| Thickness | 330 microns | 13.0 mil | |
|
3M Nextel™ XN-513 Woven Fabric 720