| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA) | 
| Manufacturer | Arkema | 
| Trade Name | Pebax® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Dry).pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | |
| Water Absorption | 0.90 % | 0.90 % | |
| Moisture Absorption at Equilibrium | 0.60 % | 0.60 % | Humidity Absorption | 
| Melt Flow |           6.0           g/10 min           @Load 1.00 kg, Temperature 235 °C  | 
                  6.0           g/10 min           @Load 2.20 lb, Temperature 455 °F  | 
        
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D | 70 | 70 | |
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min | 
| Elongation at Break | >= 50 % | >= 50 % | Nominal Strain; 50 mm/min | 
| Elongation at Yield | 22 % | 22 % | 50 mm/min | 
| Tensile Modulus | 0.414 GPa | 60.0 ksi | 1 mm/min | 
| Charpy Impact Unnotched | NB | NB | |
| NB | NB | Low Temp | |
| Charpy Impact, Notched | NB | NB | |
|           0.550           J/cm²           @Temperature -30.0 °C  | 
                  2.62           ft-lb/in²           @Temperature -22.0 °F  | 
        
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 172 °C | 342 °F | 10°C/min | 
| Flammability, UL94 |           HB                     @Thickness 1.60 mm  | 
                  HB                     @Thickness 0.0630 in  | 
        |
|           HB                     @Thickness 3.10 mm  | 
                  HB                     @Thickness 0.122 in  | 
        
| Optical Properties | Metric | English | Comments | 
|---|---|---|---|
| Transmission, Visible | 80 % | 80 % | Mfr. reports 'Transparent' but doesn't quantify. |