3M Dyneon™ FE 5620Q Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M Dyneon™ FE 5620Q Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Dyneon™ Fluoroelastomer FE 5620Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, FE 5620Q should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks display excellent processing characteristics and storage stabilityComposition: Di-polymer of vinylidene fluoride and hexafluoropropyleneLow viscosity version of FE 5640QProcess targets: injection and transfer molding, extrusion and calenderingImproved scorch resistance at high molding temperaturesProprietary incorporated cure technologyExcellent mold release-can be used in automated injection molding equipmentImproved cure technology resulting in more consistent part size from successive molding cyclesClean runningCompounds prepared from Dyneon FE 5620 can be formulated to meet Mil-R-83248Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
Mooney Viscosity 23

@Temperature 121 °C
23

@Temperature 250 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 15.4 MPa
2240 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 195 %
195 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 0.00655 GPa
0.950 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 13 %
13 %
Aged 70 hours @ 200°C, -214 O-rings; ASTM D395 Method B
Thermal Properties Metric English Comments
Transformation Temperature -18.0 °C
-0.400 °F
TR10; ASTM D1329
Component Elements Properties Metric English Comments
Fluorine, F 65.9 %
65.9 %
Descriptive Properties Value Comments
Color Opaque Off-White
MH, Maximum Torque 21 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
22.1 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ML, Minimum Torque 0.5 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
0.8 inch-lb
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
Solubility Ketones and Esters
t`50, Time to 50% cure 0.9 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
2.7 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t`90 - Time to 90% cure 1.1 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
3.7 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ts2 - Time to 2 in-lb rise from min 0.8 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 200°C, ASTM D5289
2.2 minutes
100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289