Material Notes:
This compound consists of a mixture of 50% stainless steel blended with PTFE.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 3.40 g/cc
3.40 g/cc
ASTM D4745
Bulk Density 0.800 g/cc
0.0289 lb/in³
ASTM D4745
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.1 MPa
3200 psi
ASTM D4745
Elongation at Break 210 %
210 %
ASTM D4645