Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dynamar™ RC 5115 Rubber Curative

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer 3M
Trade Name Dynamar™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dynamar™ RC 5115 Rubber Curative.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Dynamar™ Rubber Curatives RC 5105, RC 5110, RC 5115, RC 5120 and RC 5125 are liquid curatives that offer fast and easy incorporation into solvent based FKM solution coatings. RC 5115 is 50% bisphenol AF crosslinking agent in ethanol. Features and Benefits:FKM curatives for use in solvent based solution coatings Fast incorporation of curativesExcellent curative dispersion characteristics3M technical service available for developing compound formulationsInformation provided by 3M
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Viscosity <= 100 cP
<= 100 cP
Descriptive Properties Value Comments
Active Ingredients 0.5
Color Pinkish
Form Transpaent Liquid
Solubility Methanol and Ethanol
Users viewing this material also viewed the following: