3M 9740 Double Coated Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9740 Double Coated Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. This adhesive system allows for superior bonding and conformability to irregular as well as flat surfaces, and bonds well to most substrates including most low surface energy plastics. Performance grade splicing tape for corrugators and other high temperature splicing applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Carrier
38.1 microns
1.50 mil
Tape
38.1 microns
1.50 mil
Tape
88.9 microns
3.50 mil
Total (excluding liner)
Mechanical Properties Metric English Comments
Peel Strength 0.82172 kN/m
4.6875 pli
to Steel, Initial, 12 in/min
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 219 °C
426 °F
Minimum Service Temperature, Air -12.0 °C
10.4 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Carrier Polyester
Adhesive Type Acrylic
Appearance Clear
Liner 55# DK