| Category | Polymer , Adhesive |
| Manufacturer | 3M |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | 3M 9731RW Double Coated Tape.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 25.4 microns | 1.00 mil | Carrier |
| 40.6 microns | 1.60 mil | Backside Adhesive | |
| 73.7 microns | 2.90 mil | Faceside Adhesive | |
| 73.7 microns | 2.90 mil | Faceside Liner | |
| 107 microns | 4.20 mil | Backside Liner | |
| 140 microns | 5.50 mil | Total Thickness |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | 0.42729 kN/m | 2.4375 pli | ABS, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330 |
| 0.438 kN/m | 2.50 pli | Stainless Steel, 90°, Silicone Adhesive, 15 min RT; ASTM D3330 | |
| 0.438 kN/m | 2.50 pli | Polypropylene, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330 | |
| 0.4602 kN/m | 2.625 pli | Stainless Steel, 90°, Silicone Adhesive, 72 hr RT; ASTM D3330 | |
| 0.4602 kN/m | 2.625 pli | Polycarbonate, 180°, 2 mil al foil, Silicone Adhesive, 72 hr RT; ASTM D3330 | |
| 0.482 kN/m | 2.75 pli | Polypropylene, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330 | |
| 0.526 kN/m | 3.00 pli | Stainless Steel, 90°, Silicone Adhesive, 72 hr at 150°F; ASTM D3330 | |
| 0.657 kN/m | 3.75 pli | Polycarbonate, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330 | |
| 0.77789 kN/m | 4.4375 pli | Stainless Steel, 90°, Acrylic Adhesive, 15 min RT; ASTM D3330 | |
| 0.8108 kN/m | 4.625 pli | ABS, 180°, 2 mil al foil, Acrylic Adhesive, 72 hr RT; ASTM D3330 | |
| 1.0189 kN/m | 5.8125 pli | Stainless Steel, 90°, Acrylic Adhesive, 72 hr RT; ASTM D3330 | |
| 1.3257 kN/m | 7.5625 pli | Stainless Steel, 90°, Acrylic Adhesive, 72 hr at 150°F; ASTM D3330 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 121 °C | 250 °F | Long term |
| 177 °C | 351 °F | Short term |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 2.60e+15 ohm-cm | 2.60e+15 ohm-cm | Silicone Adhesive Surface |
| 3.40e+15 ohm-cm | 3.40e+15 ohm-cm | Volume | |
| 7.40e+15 ohm-cm | 7.40e+15 ohm-cm | Acrylic Adhesive Surface | |
| Dielectric Strength | 315 kV/mm | 8000 kV/in | ASTM D1000 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 18.0 Month | 18.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Backside liner | |
| Faceside Liner | ||
| Liner | Fluoropolymer non-silicone clear, PET | |
| Tan, Polycoated Kraft |