Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron DL 460E SB Latex

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 460E SB Latex.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Performance Features: Excellent alkaline stability, excellent adhesion and strengthApplications: 2K Cementious, Grouts and Modified ConcreteEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 48.5 %
48.5 %
pH 11
11
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 14.0 °C
57.2 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved