3M 7940 Aluminum Foil Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M 7940 Aluminum Foil Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 7801, 7940 and 7942 utilize 3M™Adhesive 320 which offers excellent adhesion to a variety of surfaces including high surface energy (HSE) and low surface energy (LSE) plastics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 43.2 microns
1.70 mil
Adhesive
50.8 microns
2.00 mil
Facestock
170 microns
6.70 mil
Liner
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
10.0 °C
50.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 320 High Ten Acrylic
Liner 90# Polyctd.