3M 7035 Screen Printable Polyester Performance LabelProducts

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7035 Screen Printable Polyester Performance LabelProducts.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label stocks utilize 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings, and slightly oily metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Adhesive
50.8 microns
2.00 mil
Facestock
178 microns
7.00 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method
0.614 kN/m
3.50 pli
Polypropylene, 180° Peel, 12"/min., 1" wide sample; TLMI Method
0.614 kN/m
3.50 pli
Polycarbonate, 180° Peel, 12"/min., 1" wide sample; TLMI Method
0.736 kN/m
4.20 pli
Stainless Steel, 180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
50.0 °C
122 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 350
Liner 90# Polyctd.