Material Notes:
3M™ 5640 and 5650 Series Quick Term II Silicone Rubber Termination Kits are one-piece Cold Shrink™ terminations for Jacketed Concentric Neutral (JCN) power cable. They meet the requirements of IEEE standards 48-1990, for class I terminations. In addition they meet German standard VDE 0278 parts 5 & 100, British standard A-B-N-T-9314. Similar terminations using Quick Term II technology meet French EdF standards HN 33-E-01 and HN 41-E-01. The 3M Quick Term II consists of a high dielectric constant (high-K) stress control tube insulated with a molded silicone skirted insulator. There is a four skirt design rated 15 kV, a six skirt design rated 25/28 kV and eight skirt design rated 34.5 kV. Each insulator design incorporates an extended base feature which when combined with mastic ensures a seal at the cable jacket end where the cable neutral wires are brought out. Quick Term II terminations are provided in an expanded state, mounted on a removable inner supporting plastic core. As supplied in this pre-stretched condition the termination is ready for field installation. During installation the core is unwound, allowing termination to shrink and form a tight seal. Collectively, these termination kits cover cables with primary insulation OD from 0.637” to 2.30” (16.2-58.4 mm) and with cable jacket OD from 0.93”-2.75” (23.6-70.0 mm). These kits can be used to terminate Jacketed Concentric neutral (JCN) power cables from: 4 AWG to 2000 kcmil at 15 kV, 2 AWG at 1750 kcmil at 25 kV and 1 AWG to 1500 kcmil at 34.5 kV.Information provided by 3M
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.27 MPa
1200 psi
Silicone Rubber Insulator; ASTM D42
9.611 MPa
1394 psi
EPDM Rubber Hi-K Stress Control Tube; ASTM D42
Electrical Properties Metric English Comments
Dielectric Constant 2.7

@Temperature 130 °C
2.7

@Temperature 266 °F
Silicone Rubber Insulator; ASTM D150
3.0

@Temperature 90.0 °C
3.0

@Temperature 194 °F
Silicone Rubber Insulator; ASTM D150
3.4

@Temperature 23.0 °C
3.4

@Temperature 73.4 °F
Silicone Rubber Insulator; ASTM D150
20

@Frequency 100000 Hz
20

@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
24

@Frequency 10000 Hz
24

@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
29

@Frequency 1000 Hz
29

@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
35

@Frequency 150 Hz
35

@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
24.5

@Frequency 60.0 Hz,
Temperature 65.0 °C
24.5

@Frequency 60.0 Hz,
Temperature 149 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
25.2

@Frequency 60.0 Hz,
Temperature 90.0 °C
25.2

@Frequency 60.0 Hz,
Temperature 194 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
25.7

@Frequency 60.0 Hz,
Temperature 23.0 °C
25.7

@Frequency 60.0 Hz,
Temperature 73.4 °F
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
27.2

@Frequency 60.0 Hz,
Temperature 65.0 °C
27.2

@Frequency 60.0 Hz,
Temperature 149 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
27.7

@Frequency 60.0 Hz,
Temperature 90.0 °C
27.7

@Frequency 60.0 Hz,
Temperature 194 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
28.8

@Frequency 60.0 Hz,
Temperature 23.0 °C
28.8

@Frequency 60.0 Hz,
Temperature 73.4 °F
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
Dielectric Strength 20.0 kV/mm

@Thickness 0.190 mm
507 kV/in

@Thickness 0.00750 in
Silicone Rubber Insulator; ASTM D149
Dissipation Factor 0.12

@Frequency 100000 Hz
0.12

@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.14

@Frequency 10000 Hz
0.14

@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.15

@Frequency 1000 Hz
0.15

@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.16

@Frequency 150 Hz
0.16

@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.093

@Thickness 1650 mm,
Frequency 60.0 Hz
0.093

@Thickness 65.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
0.096

@Thickness 584 mm,
Frequency 60.0 Hz
0.096

@Thickness 23.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
0.132

@Thickness 2290 mm,
Frequency 60.0 Hz
0.132

@Thickness 90.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150
0.161

@Thickness 2290 mm,
Frequency 60.0 Hz
0.161

@Thickness 90.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.165

@Thickness 1650 mm,
Frequency 60.0 Hz
0.165

@Thickness 65.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
0.166

@Thickness 584 mm,
Frequency 60.0 Hz
0.166

@Thickness 23.0 in,
Frequency 60.0 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150
Track Resistance 3600 sec
3600 sec
3.5 kV; ASTM 2303
36000 sec
36000 sec
2.5 kV; ASTM 2303