3M 4492W Double Coated Polyethylene Foam Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4492W Double Coated Polyethylene Foam Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces including polyethylene and polypropylene. 3M™ Double Coated Polyethylene Foam Tapes 4492G, 4492W, 4492B, 4496W and 4496B combine a conformable closed cell foam with a high strength acrylic adhesive that provides good initial tack and offers high ultimate adhesion to a wide variety of surfaces.Information provided by 3M
Physical Properties Metric English Comments
Density 0.0960 g/cc
0.00347 lb/in³
Thickness 20.3 microns
0.800 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.415 MPa
60.2 psi
Dynamic, 1 in.<sup>2</sup> (6.45 cm<sup>2</sup>) overlap Jaw Speed 0.5 in./min (12.7 mm/min.); ASTM D-897
Peel Strength 1.40 kN/m
8.00 pli
90° Angle Peel 12 in./min. Jaw Speed (308 mm/min.) 72 hour Dwell; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Long Term
82.0 °C
180 °F
Short Term
Descriptive Properties Value Comments
Adhesive Type 430
Liner Closed Cell Crosslinked Polyethylene Foam