Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 4056 Double Coated Urethane Foam Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4056 Double Coated Urethane Foam Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive system for bonding to various types of surfaces for mounting, joining and holding.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Release Liner
826 microns
32.5 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.345 MPa
50.0 psi
T Block, 1 in<sup>2</sup> (6.45 cm<sup>2</sup>) Jaw Speed 2 in/min (50 mm/min)
0.965 MPa
140 psi
Elongation at Break 100 %
100 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.0360 W/m-K
0.250 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 104 °C
219 °F
Long Term
193 °C
379 °F
Short Term
Electrical Properties Metric English Comments
Dielectric Strength 7.87 - 11.8 kV/mm
200 - 300 kV/in
Descriptive Properties Value Comments
Adhesive Type 100
Liner Polyurethane Foam