Exxon Chemical
Exxon Chemical > Polypropylene, Impact Modified; Molded/Extruded
Manufacturer :
Exxon Chemical
>
Category :
Polypropylene, Impact Modified; Molded/Extruded
Product List
Tips:
Up to 100 items are displayed.
PRODUCT NO.
Category
Trade Name
ExxonMobil AP03B Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil AP3N Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7011L1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7032E2 Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7033E2 Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7033L1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7033N Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7043L1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7054L1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7075L1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7085E1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP8013L1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PPU0009F Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil AP3AW Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7684KN Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7064L1 Polypropylene Impact Copolymer
Polypropylene, Impact Modified; Molded/Extruded