Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | ASTM D257 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Volume Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | ASTM D257 |
Zeus FEP Tubing FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua.. |
|||
Volume Resistivity | 1.00e+16 - 1.00e+18 ohm-cm | 1.00e+16 - 1.00e+18 ohm-cm | ASTM D257 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Volume Resistivity | 1.00e+16 - 1.00e+18 ohm-cm | 1.00e+16 - 1.00e+18 ohm-cm | ASTM D257 |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |
|||
Volume Resistivity | 1.00e+16 - 1.00e+18 ohm-cm | 1.00e+16 - 1.00e+18 ohm-cm | ASTM D257 |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |
|||
Volume Resistivity | 1.00e+17 - 1.00e+18 ohm-cm @Temperature 23.0 °C |
1.00e+17 - 1.00e+18 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers VESPEL TP-8054 Polyimide DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi.. |
|||
Volume Resistivity | 1.00e+17 - 1.00e+18 ohm-cm @Temperature 23.0 °C |
1.00e+17 - 1.00e+18 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers VESPEL TP-8161 Polyimide DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environm.. |
|||
Volume Resistivity | 1.00e+17 - 1.00e+18 ohm-cm @Temperature 23.0 °C |
1.00e+17 - 1.00e+18 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers VESPEL TP-8169 Polyimide DuPont Vespel TP-8169 parts are specified for high-temperature applications. TP-8169 parts offer a unique balance of mechanical and thermal properties for high performance in aggressive environments.. |
|||
Volume Resistivity | 1.00e+17 - 1.00e+18 ohm-cm | 1.00e+17 - 1.00e+18 ohm-cm | ASTM D257 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |