Polymer Property : Volume Resistivity = 1.00e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
IEC 60093
Raschig Group 3505 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
ASTM D257
PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
ASTM D257
PolyOne Therma-Tech™ SF-5000C TC Polyphenylene Sulfide (PPS)  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+15 - 1.00e+16 ohm-cm

@Temperature 73.4 °F
ASTM D257
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts
Superior chemical property, very high radiation resistance, electrical and thermal property, low outgassing and superior physical propertyInformation provided by Daelim H&L
Volume Resistivity 1.00e+13 - 1.00e+16 ohm-cm
1.00e+13 - 1.00e+16 ohm-cm
Potters Industries Spheriglass® 3000E Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..