Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | ASTM D257-99 |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | ASTM D257-99 |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | ASTM D257-99 |
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | ASTM D257-99 |
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | 85°C for 1,000 hrs with 85% RH; JIS-K 6249; ASTM D257 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | Conditioned; IEC 60093 |
Lanxess Durethan® DP BKV 60 H2.0 EF 900116 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, low viscosity, good flowability (Easy Flow), good heat-resistanceApplication Examples: gearbox housings, spring holders, automotive door handles |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | ASTM D247 |
Plenco 2571 Phenolic, Granular, Compression Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | IEC 60093 |
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | IEC 60093 |
Unitika A1030BRL PA6, Conditioned Information provided by Unitika Ltd. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | IEC 60093 |
Unitika A1030FR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | IEC 60093 |
Unitika A1030JR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | ASTM D247 |
Plenco 6990 Phenolic, Briquette, Compression Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Volume Resistivity | 8.00e+11 ohm-cm | 8.00e+11 ohm-cm | IEC 60093 |
Unitika A1030SR PA6, Conditioned Information provided by Unitika Ltd. |