Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | STN 34 6460 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 60093:1980-01 |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 60093 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 60093 |
Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber PA 66, injection molding 30% glass fibers, UL 94 V-0 at 0.4 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, free from halogen and red phosphorous |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | d.a.m.; IEC 60093 |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF25 IM HS L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF20 IM2 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedTPCI# 633.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3105 Polybutylene Terephthalate (PBT), Standard, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
Tra-Con Tra-Bond 2222 One-Part Surface Mount Epoxy Adhesive TRA-BOND 2222 is a solvent-free, one-part thixotropic, epoxy adhesive recommended for SMD (Surface Mount Device) bonding and sealing applications where its easy handling, high strength and superior .. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
Dow Corning SC 102 White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
Dow Corning SE 4422 SILICONE RTV One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
Dow Corning SILASTIC® 9280/60E KIT PARTS A&B 75 Shore A hardness, two-part, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Volume Resistivity | <= 5.00e+15 ohm-cm | <= 5.00e+15 ohm-cm | |
Cytec (Conap) FR-1273 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Volume Resistivity | >= 5.00e+15 ohm-cm | >= 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack LDPE SheathingInformation provided by Fainplast.. |
|||
Volume Resistivity | >= 5.00e+15 ohm-cm | >= 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Ethylplus 623 HD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack HDPE SheathingInformation provided by Fainplast.. |
|||
Volume Resistivity | >= 5.00e+15 ohm-cm | >= 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HFX 509/1 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds |
|||
Volume Resistivity | >= 5.00e+15 ohm-cm | >= 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HFX 521 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Oil resistant sheathingInformation provided by Fainplast C.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm @Thickness 3.00 mm |
5.00e+15 ohm-cm @Thickness 0.118 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm @Temperature 60.0 °C |
5.00e+15 ohm-cm @Temperature 140 °F |
IEC 60093 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm @Temperature 20.0 °C |
5.00e+15 ohm-cm @Temperature 68.0 °F |
IEC 60093 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | Cured property; ASTM D257 |
Aptek 6103-A/B Epoxy Encapsulant Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.Part A is deep red. Part B is clear to pale yellow.Information provided.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 93 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 60093 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |