Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | Test 2 |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | |
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | |
Momentive Performance Materials TSE3941 Flame Retardant Adhesive Sealant, White TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 225F PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 216 PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 216 NATURAL FA PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 100 °C |
4.00e+14 ohm-cm @Temperature 212 °F |
|
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 100 °C |
4.00e+14 ohm-cm @Temperature 212 °F |
|
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 100 °C |
4.00e+14 ohm-cm @Temperature 212 °F |
|
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrica.. |
|||
Volume Resistivity | >= 4.00e+14 ohm-cm | >= 4.00e+14 ohm-cm | ASTM-D1829 |
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film Applications: thick films and lasers |
|||
Volume Resistivity | <= 4.00e+14 ohm-cm | <= 4.00e+14 ohm-cm | |
Cytec (Conap) FR-1200 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | <= 4.00e+14 ohm-cm | <= 4.00e+14 ohm-cm | |
Cytec (Conap) FR-1210 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 23.0 °C |
4.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FRT 95 Flexible PVC, Insulation Telephone and interphone cables |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | |
Dow Corning 3-6512 A&B ELASTOMER Two-part, transparent, 1:1, moderate heat cure, long pot life, cures to soft elastomer.Information provided by Dow Corning |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | Cured property; ASTM D257 |
Aptek 7503LM-PMF UV Urethane Conformal Coating UV-cured, low modulus, shadow cures under components. Excellent adhesion without primer. Repairable. Qualified to MIL-I-46058C, types UR and AR. Castable version – UVIKOTE 7504 LM-PMF.Information p.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | Cured property; ASTM D257 |
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.Information provided by Aptek Laboratories, .. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | |
Aremco Aremco-Bond™ 526N High Performance Epoxide Clear-Amber, 1:1 System for Tough Bonding Applications Also available filled with aluminum oxide (Alumina) or pigments |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | DIN 53 482, VDE 0303, Part 3 |
Hippe PVDF Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 23.0 °C |
4.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds KL 96/1 Flexible PVC, Insulation for High Temperatures Lead Free Automotive cables low thickness |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | Test 2 |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 23.0 °C |
4.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FKA 97 Flexible PVC, Flame Retardant Insulation Lead Free Telephonic insulation |
|||
Volume Resistivity | 4.00e+14 ohm-cm | 4.00e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |