Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.50e+14 ohm-cm | 7.50e+14 ohm-cm | |
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Volume Resistivity | 7.50e+14 ohm-cm | 7.50e+14 ohm-cm | |
Tra-Con Tra-Cast 3109 Low Cost Epoxy Casting System TRA-CAST 3109 is a versatile epoxy casting system developed for solvent-free production casting, potting, encapsulating, and coating applications where low cost, easy handling and flowability, and e.. |
|||
Volume Resistivity | 7.50e+14 ohm-cm | 7.50e+14 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |
|||
Volume Resistivity | 7.50e+14 ohm-cm | 7.50e+14 ohm-cm | Cured property; ASTM D257 |
Aptek 6550-A/B Epoxy Encapsulant High thermal conductivity, microelectronic grade blob-top encapsulant. Ultra high purity. Excellent heat and moisture protection for sensitive chips/circuitry. Premixed frozen syringes available for.. |