Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | STN 34 6460 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 60093 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | d.a.m.; IEC 60093 |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF20 IM2 BK 20% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF25 IM HS L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF25 IM L 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF33 IM L UV 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier, Lubricant and UV StabilizerFeatures: Good UV Resistance, Impa.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF20 IM2 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedTPCI# 633.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
Dow Corning SC 102 White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
Dow Corning SE 4422 SILICONE RTV One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | |
Dow Corning SILASTIC® 9280/60E KIT PARTS A&B 75 Shore A hardness, two-part, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Volume Resistivity | <= 5.00e+15 ohm-cm | <= 5.00e+15 ohm-cm | |
Cytec (Conap) FR-1273 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 1002YB Wire & Cable Linear Low Density Polyethylene Resin Product Description: LL 1002YB is a C4 Ziegler Natta LLDPE for Low Voltage power cable and Telecom jacketing. The grade contains a higher level of antioxidants and has excellent Environmental Stress.. |
|||
Volume Resistivity | >= 5.00e+15 ohm-cm | >= 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack LDPE SheathingInformation provided by Fainplast.. |
|||
Volume Resistivity | >= 5.00e+15 ohm-cm | >= 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Ethylplus 623 HD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack HDPE SheathingInformation provided by Fainplast.. |
|||
Volume Resistivity | >= 5.00e+15 ohm-cm | >= 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HFX 509/1 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds |
|||
Volume Resistivity | 5.00e+15 ohm-cm @Temperature 60.0 °C |
5.00e+15 ohm-cm @Temperature 140 °F |
IEC 60093 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm @Temperature 20.0 °C |
5.00e+15 ohm-cm @Temperature 68.0 °F |
IEC 60093 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | Cured property; ASTM D257 |
Aptek 6103-A/B Epoxy Encapsulant Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.Part A is deep red. Part B is clear to pale yellow.Information provided.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 93 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | 3.30 mm; ASTM D257 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | ASTM D257 |
PolyOne Edgetek® SF-35GF-25MN/000 L Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 5.00e+15 ohm-cm | 5.00e+15 ohm-cm | IEC 60093 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |