Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4000 ohm-cm | 4000 ohm-cm | This value is measured for the pure EPOCYL NC R2HM-01, without any fiber reinforcements. |
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the.. |
|||
Volume Resistivity | 4000 ohm-cm | 4000 ohm-cm | |
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers PREGCYL™ NC R2HM-01 is a pre-impregnated material based on our EPOCYL NC R2HM01 formulated epoxy resin system modified with our own Carbon Nanotubes (CNT) and specifically developed to enhance the .. |
|||
Volume Resistivity | 4000 ohm-cm | 4000 ohm-cm | |
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Volume Resistivity | 4000 ohm-cm | 4000 ohm-cm | |
LATI Latistat 66-06 PA66 Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Volume Resistivity | 4000 ohm-cm | 4000 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Volume Resistivity | 4000 ohm-cm | 4000 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Volume Resistivity | 4000 ohm-cm | 4000 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |