Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific) Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® 193 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® 194 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® 4704 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FL903 PC Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm). |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FL920 PC Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® PPC4701 PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® PPC4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FL900 PC Lexan* resin FL900 is a Br- & Cl-free flame retardant grade that can be foamed for weight reductions. UL-94 V1 listed at 3.9mm together with good stiffness, heat, creep and impact performance make i.. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® FL920 PC (Asia Pacific) Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
Volume Resistivity | >= 2.50e+17 ohm-cm | >= 2.50e+17 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Volume Resistivity | 2.50e+17 ohm-cm | 2.50e+17 ohm-cm | ASTM D257 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Volume Resistivity | 2.50e+17 ohm-cm @Temperature 20.0 °C |
2.50e+17 ohm-cm @Temperature 68.0 °F |
|