Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 85U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | 70°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-d Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | 150°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | |
Momentive Performance Materials RTV159 High Strength Silicone Adhesive Sealant, Red RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | IEC 60167 |
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and.. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | |
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | |
Dow Corning 4 ELECTRICAL INSULATING COMPOUND Silicone-based compound, moderate consistency. Lubricant suitable for electrical connectors and joints.Information provided by Dow Corning |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance.. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d.. |
|||
Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | ASTM D247 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |