Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 37.0 kV/mm | 940 kV/in | |
Ineos ABS Lustran® H950 Very high heat resistance,,Property data per ISO test methods. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | NF EN 60243.1 |
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | ASTM D149 |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Dielectric Strength | 37.0 kV/mm @Thickness 1.50 mm |
940 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | |
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |
|||
Dielectric Strength | 37.0 kV/mm @Thickness 1.50 mm |
940 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | K20/P50; IEC 60243-1 |
Styrolution Terlux® 2812 HD MABS Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Dielectric Strength | 37.0 kV/mm @Thickness 1.00 mm |
940 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika A1030FR PA6, Dry Information provided by Unitika Ltd. |
|||
Dielectric Strength | 37.0 kV/mm @Thickness 1.00 mm |
940 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Unitika A1030JR PA6, Dry Information provided by Unitika Ltd. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | Under ambient atmosphere; ASTM D149 |
Unitika UNILATE® 1 PC PET Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50 Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is .. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BG-15 PA6-GF15 Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BG-30 FC PA6-GF30 Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface .. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-40 FC PA6-GF40 Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BT 40 Z PA6 Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33 Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30 Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4181 black PA1010 Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly .. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4181 nat PA1010 Product description: Grilamid XE 4181 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 natural is highly resist.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BGZ-40 PA6-GF40 Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | Arlon SQA-TMS-020 |
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 |
BASF Ultraform® N2650 Z6 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |