| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | 1000 V/sec; ASTM D149 |
|
SABIC 318CN Linear Low Density Polyethylene for Wire & Cable
Product Description: 318CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock a..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | |
|
Saint-Gobain Quartzel® Fused Quartz Textiles
Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 |
|
Styrolution Terluran® GP-22 ABS
Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and..
|
|||
| Dielectric Strength |
37.0
kV/mm @Thickness 1.00 mm |
940
kV/in @Thickness 0.0394 in |
IEC 60243-1 |
|
Unitika A1030JR PA6, Dry
Information provided by Unitika Ltd.
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | Under ambient atmosphere; ASTM D149 |
|
Unitika UNILATE® 1 PC PET
Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | cond; IEC 60243-1 |
|
DSM EcoPaXX® Q-X07209 PA410-I-GF40
% Glass Reinforced, Impact Modified
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I
Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I
Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I
Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I
Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is ..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I
Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® BG-15/2 PA6-GF15
Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® BG-30 FC PA6-GF30
Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface ..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® BG-30/2 PA6-GF30
Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® BG-40 S PA6-GF40
Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33
Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | dry; IEC 60243-1 |
|
EMS-Grivory Grivory® XE 4155 black 9992 PA612-I
Information provided by EMS Grivory
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30
Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® BG-50 S PA6-GF50
Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | conditioned; IEC 60243-1 |
|
EMS-Grivory Grivory® XE 5051 (BGZ-40 FC) PA6-GF40
Product description: Grilon XE 5051 is a impact modified, heat stabilized PA 6 injection molding grade with 40% glass fiber reinforcement. Grilon XE 5051 has the following important properties: High..
|
|||
| Dielectric Strength | 37.0 kV/mm | 939 kV/in | ASTM D149 |
|
Arlon 51581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 |
|
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 |
|
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | Arlon SQA-TMS-020 |
|
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 |
|
BASF Ultraform® N2650 Z6 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 |
|
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | IEC 60243-1 3 |
|
BASF Ultrason S 6010 PSU
Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (..
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | K20/P50; IEC 60243-1 |
|
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN
Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Dielectric Strength | 37.0 kV/mm | 940 kV/in | ASTM D149 |
|
PolyOne Geon™ Vinyl Wire & Cable W2402 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||