Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 31.5 kV/mm @Thickness 1.60 mm |
800 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Dielectric Strength | 31.5 kV/mm @Thickness 1.60 mm |
800 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Dielectric Strength | 31.5 kV/mm @Thickness 1.60 mm |
800 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | Short Time; 1/8 inch; ASTM D149 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer Notes: Non-halogenated; RoHS Compliant; MBDC: Green Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General .. |
|||
Dielectric Strength | >= 31.5 kV/mm | >= 800 kV/in | At 40 mils; ASTM D149 |
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 mas.. |
|||
Dielectric Strength | 31.5 - 66.9 kV/mm | 800 - 1700 kV/in | ASTM D149 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | |
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. I.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | |
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | Arlon SQA-TMS-020 |
Arlon P31000A005 0.005" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D295 |
3M Scotch® 2510 Varnished Cambric Tape Scotch® Varnished Cambric Tapes are made from straight-cut woven cotton cambric fabric. The fabric is oil primed and coated with a high-grade yellow electrical insulating varnish. Varnished cambric.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | Standard Conditioning; ASTM D4325 |
3M Scotch™ 23 Rubber Splicing Tape Scotch® Rubber Splicing Tape 23 is a highly conformable, self-fusing EPR (Ethylene Propylene Rubber) based, high voltage splicing tape. It is a non-vulcanizing, shelf-stable tape with excellent ele.. |
|||
Dielectric Strength | 31.5 - 43.3 kV/mm | 800 - 1100 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon R38095R011 0.011" (0.279 mm) Partially Cross Linked Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Partially Cross Linked Silicone RubberSubstrate: Style 1528 Fiberglass:Side 2: Partially Cross Linked Silicone Rubber Product Use: Electrical InsulationAppearance: Red si.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | |
3M EPS-200 Tubing 3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special the.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D295 |
3M Scotch® 2520 Varnished Cambric Tape Scotch® Varnished Cambric Tapes are made from straight-cut woven cotton cambric fabric. The fabric is oil primed and coated with a high-grade yellow electrical insulating varnish. Varnished cambric.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | |
3M VFP-876 Tubing 3M VFP-876 is the most flexible of the heat-shrinkable, polyolefin tubings. Rated at 135°C. VFP-876 Tubing has been engineered to offer a low shrink temperature of 100°C. This allows the tubing to.. |
|||
Dielectric Strength | 31.5 - 43.3 kV/mm | 800 - 1100 kV/in | ASTM D149 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |
|||
Dielectric Strength | 31.5 kV/mm | 800 kV/in | ASTM D149 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |