Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 22 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 24 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® F 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® FC 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Lanxess Pocan® B 4215 000000 PBT, 12% Glass Fiber PBT, 12% glass fibers, injection molding, flame retardant |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243-1 |
Mitsubishi Xantar® G6F 23 UR Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | VDE 0303/4 |
Polyram RamSter PF320G2 PBT, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | VDE 0303/4 |
Polyram RamSter PF320G3 PBT, 15% Glass Fiber, Flame Retardant 15% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | |
Covestro Baygal® 90 IK 51 Polyurethane Uses: Suitable for the solid insulation of measuring transducers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its ne.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® 410 Paper, 25.5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BK-30 PA6-GB30 Information provided by EMS Grivory |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 240Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 340Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | ASTM D149 |
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry) Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl.. |
|||
Dielectric Strength | 29.0 kV/mm @Thickness 2.00 mm |
737 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® 100Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROCARB Polycarbonate CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain.. |
|||
Dielectric Strength | 29.0 kV/mm | 737 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TS FR PA666 FR Information provided by EMS Grivory |