Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 44.0 kV/mm | 1120 kV/in | |
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Dielectric Strength | 44.0 kV/mm | 1120 kV/in | IEC 60243-1 |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Dielectric Strength | 44.0 kV/mm | 1120 kV/in | IEC 60243-1 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Dielectric Strength | >= 44.0 kV/mm | >= 1120 kV/in | Breakdown |
Advanced Ceramics ACL 2088 Zinc Alumino-Silicate A low expansion glass-ceramic suitable for sealing to molybdenum.Information provided by Advanced Ceramics Limited (ACL) |
|||
Dielectric Strength | 44.0 kV/mm | 1120 kV/in | IEC 60243-1 |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Dielectric Strength | >= 44.2 kV/mm | >= 1120 kV/in | |
Caplinq LINQTAPE™ PIT1A Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p.. |
|||
Dielectric Strength | >= 44.2 kV/mm | >= 1120 kV/in | |
Caplinq LINQTAPE™ PIT1S Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p.. |
|||
Dielectric Strength | 44.1 kV/mm | 1120 kV/in | ASTM D149 |
Unitika U-8000 U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |