Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.5 kV/mm | 520 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1030HL Nylon 6/6
(discontinued **) Available in North America Filler: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: GM GMW3038P-PA.. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Dielectric Strength | 20.5 kV/mm @Thickness 1.91 mm |
521 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials RTV6136 Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Dielectric Strength | 20.5 kV/mm @Thickness 1.91 mm |
521 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials RTV6156 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Dielectric Strength | 20.5 kV/mm @Thickness 1.91 mm |
521 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials RTV6166 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF30 FR-N 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PBT GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: Natural ColorTPCI# 8649111Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 9864111Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP E GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled, Heat Stabilized and High Viscosit.. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PP GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® TPX-HTN-01027 A 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® TPX-PBT-01022 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedInformation provided by TP Composites, .. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant, Halogen Free and Impact ModifiedAppearance: BlackI.. |
|||
Dielectric Strength | 20.5 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
521 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
DAM; Short Time; ASTM D149 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 20.5 kV/mm | 520 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PPA GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low .. |