Polymer Property : High Voltage Arc-Tracking Rate, HVTR = 10.1 mm/min Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
Average value: 17.8 mm/min Grade Count:3
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746A
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..