Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | surface, PLC code 1; UL 746A |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 131 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 201R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 203 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 241 PC General Purpose polycarbonate with 10.5 of melt flow rate. Improved flame retardance. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 244R PC (Asia Pacific) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 915R PC (Asia Pacific) Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 915RP PC (Asia Pacific) Lexan* 915RP Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | surface, PLC code 1; UL 746A |
SABIC Innovative Plastics Lexan® FXD171R PC Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 143 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific) LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® LUX9612 PC (Asia Pacific) Lexan LUX9612 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1001 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1007 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.10 mm |
60 - 120 arcs @Thickness 0.0433 in |
UL Rating PLC 1 (60-120 arcs) |
Covestro Makrolon® 6465 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 143R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |