Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific) Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943A PC Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943AR PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943ASR PC (Asia Pacific) More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 955AU PC (Asia Pacific) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® FL920 PC Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® 151 PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 945U PC Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 955U PC (Asia Pacific) Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 0.750 mm |
30 - 60 arcs @Thickness 0.0295 in |
NC |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.50 mm |
30 - 60 arcs @Thickness 0.0591 in |
(BK, BN) |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.50 mm |
30 - 60 arcs @Thickness 0.0591 in |
BN, BK |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.57 - 6.33 mm |
30 - 60 arcs @Thickness 0.0618 - 0.249 in |
UL PLC 2 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Noryl PX5622 PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific) GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4101 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA 30% Glass Reinforced PPE+PA Alloy. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT 33 % glass reinforced, impact modified. Connectors, etc. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4020 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 925U PC Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additi.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 953A PC Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |