Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 35000 V | >= 35000 V | |
ChevronTexaco EDM Fluid Texaco EDM Fluid delivers value through:Accurate machining — Good dielectric properties provide controlled discharge characteristics. Low viscosity provides excellent fluidity through the spark gap.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe UP GM 201 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided .. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C |
>= 35000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 - 90.0 °C |
>= 35000 V @Temperature 194 - 194 °F |
Average value: 32900 V Grade Count:9 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |