Polymer Property : Dielectric Strength = 25.6 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 25.6 kV/mm

@Thickness 1.60 mm
650 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics LNP COLORCOMP NX05467 PC+ABS
LNP* COLORCOMP* NX05467 is an unfilled Polycarbont+ABS resin. Added features of this grade are: Non-Chlorinated, Non-Brominated Flame Retardant.
Dielectric Strength 25.6 kV/mm

@Thickness 3.20 mm,
Temperature 120 °C
650 kV/in

@Thickness 0.126 in,
Temperature 248 °F
Short Time; ASTM D149
DuPont Performance Polymers Rynite® RE5231 BK533 PET  (Unverified Data**)
Rynite® RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Information provided by DuPont Performance Polymers
Dielectric Strength 25.6 kV/mm

@Thickness 1.57 mm
650 kV/in

@Thickness 0.0620 in
Condition - A
Industrial Laminates/Norplex NP180 Synthetic Fabric  (discontinued **)
Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments.Thickness Tested: ..
Dielectric Strength 25.6 kV/mm

@Thickness 1.57 mm
650 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP101 Synthetic Fabric
Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp..
Dielectric Strength 25.6 kV/mm

@Thickness 1.60 mm
650 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® DR48 PBT
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.