Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 100 sec | 100 sec | |
Pyrotek TS-110 Thermoset Electrical Insulation Product (Nema Grade: G-10) Glass reinforcement, Epoxy Resin, Natural Color. High flexural, impact and bond strength at room temperature.Information provided by Pyrotek. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Shell Carilon® DP P1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr.. |
|||
Arc Resistance | 100 sec | 100 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Plenco 7300 Phenolic, Nodular, Injection Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Kolon KOPET® KP132G30VO FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Arc Resistance | 100 sec @Thickness 3.17 mm |
100 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Arc Resistance | 100 sec @Thickness 3.17 mm |
100 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP504 Glass Fabric Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax PBT 2000-201D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Arc Resistance | 100 sec | 100 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 100 sec | 100 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 100 sec | 100 sec | Practical Use (Water Absorption 2.5%); ASTM-D495 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 100 sec | 100 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 100 sec | 100 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy
(discontinued **) Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with .. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |