Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | |
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | ASTM D257 |
Ovation Polymers Nemcon™ H PC DP113/X5 Polycarbonate Polycarbonate-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | per cm square at 50% humidity; ASTM D257 |
Network Polymers PC-1029 AS/P Description: Antistatic PolycarbonateInformation provided by Network Polymers Inc. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257-91 |
NeXolve LaRC™-CP1 Polyimide Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptak.. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | VDE 0303 |
GEHR Plastics ECTFE Polyethylene Chlorotrifluoroethylene Ethylene-Chlortrifluorethylene exhibits an extraordinary impact strength at temperatures ranging from -76°C to 150°C. A great part of the product properties attributes to the very smooth surfa.. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | VDE 0303 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+12 ohm | 1e+05 - 1.00e+12 ohm | ASTM D257 |
Kostat KAH1 Heat Seal Activated Cover tapes KOSTATs KAH1 series of Heat Seal Activated Cover Tape is manufactured using Antistatic Polyethylene Terephthalate film and other proprietary adhesive materials. The component for its anti-static pr.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | 50% RH; ASTM D257 |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+12 ohm | 1.00e+12 ohm | ASTM D257 |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257 |
Quadrant EPP Quadrant CPVC - ASTM D1748, Cell Classification (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+12 ohm | >= 1.00e+12 ohm | ASTM D257 |
Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+12 ohm | 1e+05 - 1.00e+12 ohm | ASTM D257 |
PolyOne Edgetek® AM-10CF-20GF/000 HS Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |