Polymer Property : Surface Resistivity per Square = 1.00e+9 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite
Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem..
Surface Resistivity per Square 1e+05 - 1.00e+9 ohm
1e+05 - 1.00e+9 ohm
NeXolve LaRC™-CP1 Conductive Black Polyimide
Lower RF loss than other black and conductive black polyimides. NeXolve’s Conductive Black LaRC™-CP1 Polyimide is filled with carbon nanoparticles to produce a conductive black polyimide material ..
Surface Resistivity per Square 1e+05 - 1.00e+9 ohm
1e+05 - 1.00e+9 ohm
ASTM D257
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Surface Resistivity per Square 1e+05 - 1.00e+9 ohm
1e+05 - 1.00e+9 ohm
ASTM D257
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICS-1001 PET Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICS-1002 PP Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICS-1003 PS Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICS-1004 PVC Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICS-1005 ABS Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1e+05 - 1.00e+9 ohm
1e+05 - 1.00e+9 ohm
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric
Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined..
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257
Kostat BK-STAT 7048BK ABS Compound
BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline..
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257
Kostat BK-STAT 7048BK ABS Sheet
BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness ..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICD-1000 PC Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICD-1001 PET Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICD-1002 PP Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICD-1003 PS Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICD-1004 PVC Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
after 250% elongation; ASTM D257
Kostat ICP-STAT ICS-1000 PC Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257
Ensinger Tecaform™ SD Acetal (POM)
Ensinger-Hyde static dissipative acetal contains no carbon fibers or powders and is generally accepted for clean room use. With its surface resistivity of 109 to 1011 ohm/square and its excellent b..
Surface Resistivity per Square 1.00e+9 - 1.00e+14 ohm
1.00e+9 - 1.00e+14 ohm
ASTM D257
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM)
Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti..
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
IEC 60093
Arkema Group Pebax® MH 1657 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MH 1657 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 1657 is an inherently dissipative polymer and can be dry blended or compounded w..
Surface Resistivity per Square 1.00e+9 - 1.00e+12 ohm
1.00e+9 - 1.00e+12 ohm
ASTM D257
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical..
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257
Kostat BK-STAT P048BK PP Sheet
BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness ..