Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 225 V | 225 V | |
Plastcom SLOVAMID 6 GF 10 FRA 5 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 10% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Comparative Tracking Index | >= 225 V | >= 225 V | IEC 60112 |
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East) GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Comparative Tracking Index | 225 V | 225 V | ASTM D3638 |
Plenco 50030 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 112 |
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Lexan® 945A PC (Europe-Africa-Middle East) Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Comparative Tracking Index | 225 V | 225 V | UL 746A |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
Comparative Tracking Index | 225 V @Thickness 2.00 mm |
225 V @Thickness 0.0787 in |
IEC 112 |
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® 22 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® 24 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® MX 2032 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® MX 2015 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Covestro Makrolon® 6267 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Formerly Makrolon DP1-1872MVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 3.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
DSM Arnite® TV4 241 SN PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Comparative Tracking Index | 225 V | 225 V | |
Covestro Makrolon® 6870 Polycarbonate Pseudoplastic behavior and high viscosity extrusion and injection molding grade, less resistant to UV than e.g. MAKROLON 6555.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScie.. |
|||
Comparative Tracking Index | 225 V | 225 V | dry; IEC 60112 |
DSM Stanyl® TC154 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
Comparative Tracking Index | 225 V | 225 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® L 20 LF grey PA12 Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b.. |
|||
Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
Eurotec® Tecodur® PB70 GR15 BK002 XA21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black Information provided by Eurotec® |
|||
Comparative Tracking Index | 225 V | 225 V | VDE 0303-P1, IEC 112 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS Characteristics: Thermic resistant |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
DSM Arnite® TV4 440 KL PBT/PET Blend-20% Glass Reinforced (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Comparative Tracking Index | 225 V | 225 V | ASTM D3638 |
Plenco 51015 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |