Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Comparative Tracking Index | >= 225 V | >= 225 V | IEC 60112 |
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East) GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East) LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber
(discontinued **) PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® 19 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® 25 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber PBT, 7% glass fibers, injection molding, flame retardant |
|||
Comparative Tracking Index | 225 V | 225 V | UL 746 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Comparative Tracking Index | 225 V @Thickness 2.00 mm |
225 V @Thickness 0.0787 in |
IEC 60112 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Teijin Panlite® LV-2225Z Transparent and Weather Resistant grade Polycarbonate Resin Injection molding grade that is necessary to be slightly high fluidity. It has weather resistance, mold release property and is bluish-tinted to exhibit clear color.Applications:Components of electr.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Covestro Bayblend® T85 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |
|||
Comparative Tracking Index | 225 V | 225 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50 Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black Information provided by Eurotec® |
|||
Comparative Tracking Index | 225 V | 225 V | Solution A; IEC 60112 |
Eurotec® Tecotek® PC44 GR003 ZG70 PC, unfilled, flame retardant - halogen (RoHS compliant), light grey Information provided by Eurotec® |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET) Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 225 V | 225 V | UL 746A |
Chevron Phillips Ryton® R-7 02 Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R-7 02 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compound wit.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
CENTROPLAST CENTROCARB Polycarbonate CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
Mitsubishi Xantar® 27 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
SABIC Innovative Plastics Lexan® 943 PC (Europe-Africa-Middle East) LEXAN 943 is a medium viscosity flame retardant, UV-stabilized grade, especially suitable for electrical applications. |